Categories | Stainless Steel Tubing |
---|---|
Brand Name: | Y & G |
MOQ: | Negotiation |
Payment Terms: | L/C, T/T |
Supply Ability: | 8000MT/Month |
Delivery Time: | 25-35 days |
Packaging Details: | Exporting package/wooden box / per customers’ requirement |
Price: | Negotiable |
Material: | UNS S32750,S31803, S32205, S32760 |
Standard: | SA789,A790 |
Type: | Seamless,Welded |
OD: | 1/4inch~24inch |
Wall Thickness: | SCH10S , SCH10, SCH20, SCH30, SCH40S... |
Application: | Heat exchangers and coolers |
Surface Treatment: | Varnish, Oil-dip, Passivation, Phosphating, Shot Blasting |
Delivery Status: | Annealed, normalized, normalized+Tempered, etc |
Company Info. |
Y & G International Trading Company Limited |
Verified Supplier |
View Contact Details |
Product List |
SA789 UNS S32750 Stainless Steel Tubing Super Duplex Stainless Steel Pipe / Tube 25.4 * 2.11mm
Product Standard: ASME SA789
Main steel grades: UNS S32750,S31803, S32205, S32760
Application: For heat exchangers and coolers and devices that are resistant to seawater, such as high temperature and concentrated nitric acid, such as oil refining, fertilizer, papermaking, petroleum, and Foundry
Features:
1.Superior resistance to general and local corrosion, especially to stress corrosion, pitting corrosion, crevice corrosion, corrosion fatigue and abrasion & corrosion.
2.Good weldability
3.Good mechanical properties
4.Excellent intergranular corrosion resistance
5.High cost-effectiveness, long life time
Chemical Composition & Physical Properties:
Grade | C max | Si max | Mn max | P max | S max | Cr | Ni | Mo | N |
UNS S32750 | 0.030 | 0.8 | 1.2 | 0.030 | 0.015 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 |
UNS S31803 | 0.030 | 1.0 | 2.0 | 0.020 | 0.020 | 21.0-23.0 | 4.5-6.5 | 2.5-3.5 | 0.08-0.20 |
UNS S31500 | 0.030 | 1.0 | 1.2-2.0 | 0.030 | 0.030 | 18.0-19.0 | 4.5-5.5 | 2.5-3.5 | 0.05-0.10 |
Grade | Y.S.MPa min | T.S.Mpa min | Elongation % | Hardness HRC |
UNS S32750 | 550 | 800 | 15 | 20 |
UNS S31803 | 450 | 620 | 25 | 20 |
UNS S31500 | 440 | 630 | 30 | 20 |
Mark: As required.
Inspection and Test: chemical composition test, mechanical properties test(tensile, yield, elongation), process properties test(flatting, flaring, bending, hardness, impact, etc.), appearance and size test, non-destructive inspection test, hydrostastic test.
Delivery status: Annealed, normalized, normalized+Tempered, etc.
Surface treatment: oil impregnation, paint, passivation, phosphating, shot blasting etc.
Packing: Exporting package/wooden box /as requirement.